• Homogeneous PVC Flooring Commercial Flooring System 1
  • Homogeneous PVC Flooring Commercial Flooring System 2
Homogeneous PVC Flooring Commercial Flooring

Homogeneous PVC Flooring Commercial Flooring

Ref Price:
get latest price
Loading Port:
China main port
Payment Terms:
TT OR LC
Min Order Qty:
1000 m²
Supply Capability:
100000 m²/month

Add to My Favorites

Follow us:


OKorder Service Pledge

Quality Product, Order Online Tracking, Timely Delivery

OKorder Financial Service

Credit Rating, Credit Services, Credit Purchasing

Item specifice

Formaldehyde:
E0
Material:
Sandwich Panel
Feature:
Soundproof,Dust-Proof
Color:
Wood Grain
Position:
Interior
Certification:
MSDS,Fsc,Carb,CE,ISO,BS
Customized:
Non-Customized,Customized

Product Information:

 

Antistatic PVC/Vinyl Flooring

The floor uses the PVC resin as the main component, and utilizes the plastic particle interfaces to form the permanent conductive/anti-static network. The floor tile looks like the marble. It provides a good performance in the decoration projects. Abrasion resistance, corrosion resistance, long life performance, aging resistance and low dust emission are it’s features.

 

Product Advantages:

High precision on size,good wearing ability, anti-dust, anti-water,good conductivity to electricity.

Easy to install and maintenance.


Product Application:

The products are applicable to the decoration and fitment of the apparatus rooms for the industries of telecommunication, electronics, microelectronics and medicine etc, and the clean rooms or workshops for the computer or electronic instrument industries.

 

Product Specification:

ITEM

TECHNICAL DATA

THICKNESS EN426

2.0mm,2.5mm,3.0mm

SIZE EN426

600x600mm

610x610mm

WEIGHT EN430

3.8Kg/2.0mm,4.8Kg/2.5mm,5.8Kg/3.0mm

ELECTRIC PROPERTIES

DIN51953 ASTM F-150 OR NFPA99

CONDUCTIVE TILE

DISSIPATIVE TILE

10^4~10^6 ohm

10^6~10^9 ohm

DECAY TIME

SJ/T10694-2006(±1000V±100V≤2s)

EQUAL 0.4S

EQUAL 0.4S

CHARGE VOLTAGE

SJ/T10694-2006(ⅠVⅠ<100V)

EQUAL 70

EQUAL 70

FIRE RESISTANCE

DIN4102

B1

B1

COMBUSTION PROPERTIES

SJ/T11236-2001(<10S,reach FV-0)

EQUAL 0.35IFV-0

EQUAL 0.35IFV-0

AMOUNT OF ANTI WEAR

SJ/T11236-2001(≤0.020g/cm 21000r)

EQUAL0.014

EQUAL0.014

ANTI-WEAR PROPERTIES

EN660pt2

ITEN-T<2.0mm3

ITEN-T<2.0mm3

WHEEL PRESURE

EN425

No influence

No influence

RESIDUAL CONAVITY

EN433/DIN51955

0.03mm(2.0mm)

0.035mm(2.5mm)

0.04mm(3.0mm)

0.03mm(2.0mm)

0.035mm(2.5mm)

0.04mm(3.0mm)

DIMENTIONAL STABILITY

≤0.10%

≤0.10%

COLOR FASTNESS ISO105BO2

At least 6

At least 6

RESISTANCE TO CHEMICALS

DIN423/DIN51958

Offers excellent resistance ask for special sheet

Offers excellent resistance ask for special sheet

IMPACT SOUND ABSORPTION

VLI,ISO104,ISO717

Approx 2dB

Approx 2dB

STANDARD FOR HEALTH CARE FACILITIES NFPA 99

Confirms to the requirement of NFPA99 in effect at the tine of installation


 

.jpg

.jpg

Homogeneous PVC Flooring Commercial Flooring

Q:Composite wood floor with tiles which tiles which point? Composite wood flooring with the wood floor as afraid of water? If mixed with the words, the bedroom with a wooden floor good? More
Composite floor and floor tiles which depends on the use of occasions. If it is the living room, both can be used; if it is the bedroom, study, etc., the composite floor is more appropriate, more warm, tiles are blunt, relatively cold. If used in combination, the bedroom with the most appropriate wooden floor. Wood flooring is a natural material, with breathing, close to people, return to nature, can seat to sit, floor and lying, Dongnuanxialiang, used in the bedroom warm, warm, very user-friendly, composite floor and wood floor Sedan meter tamper is wood structure, so are more afraid of water, and because the structure of the reasons, the composite floor of the moisture resistance is less than solid wood flooring.
Q:I am buying 1/2 engineering flooring and I am going to put it down as a floating floor on a crawl space. My question is do I have to put down any moisture barrier or foam underneath?
Since it is above a crawl space you will want to use a some underlayment.
Q:How to lay their own composite floor
Floor heating room floor materials or the choice of floor tiles is better. This can be OKorder Geng high international 薨 uan arm for the force to ensure better heat conduction, heating up faster. Gas use is also more economical. Composite floor to be slightly worse .40 yuan compound The floor can be sure that is not a good floor. As for the floor tiles in the file on it. In order to better heat, paving in the case of ensuring the quality of the cement layer as low as possible.If there are more problems, you can click ID consultation.
Q:Have you heard that when the shop sprinkle some pepper can pest control is this? What better way? More
Composite flooring with glue. Do not have rafts to destroy the evil raccoon scratched state Shan card worry insects. As long as moisture can be. When installed around the gap to stay good. Ground level generally do not have any problems.
Q:What is the price of geothermal reinforced laminate flooring?
80-200 yuan between. It is recommended about 100 or so, no matter what brand you use the floor, remember to first ask whether there is no geothermal. And then look at the back of the board, the back raft hides to destroy the disgusting belly rub the color of the sand is the international common orange. I suggest you to look at: the elephant, nature, the couplet.
Q:Is the composite floor fading away?
The composite floor is more durable than the average wooden floor unless the long term light does not change color. The discoloration of wood is mainly caused by the absorption of ultraviolet light, wood sapwood and heartwood to absorb ultraviolet light after the degree of discoloration, matt sub-decoration will lead to pavement after the floor to produce a certain color. The resulting light color is a normal phenomenon, not a product quality problems. Therefore, after the pavement of the sun at the side of the lungs of the twist monk singing Kyrgyzstan do not long-term exposure in the sun, appropriate to take the necessary shading measures.
Q:My home is warm, has been heating, the composite floor was blisters how to do
To warm if the leak ~ repaired in the shop ~ ~ ~
Q:New house ready to decorate, is the election real 朩 floor good? Or composite floor?
Composite flooring
Q:My place where small, something more, had their own shop composite floor, do not know how to shop. Consult the knowledgeable master to help give pointers about, thank you! More
Ready to hammer, and a board, each board to fight up when there will always be gaps, with a hammer pad with a knock on the board, the raft razed the drums can not directly knock on the floor, the floor will be knocked on the floor , Skirting line, then directly with glass glue it, a simple point
Q:My house up and down the floor of the water there is not much water above the floor there is water just started with the foot of the wall on the edge of the wall will have water overflow from the wall after an hour after the top of the skeleton repair Lennon agent Yi Chuan floor now basically no It is estimated that the penetration of the floor has been in the first time to open the door to open the door which the Supreme who knows the floor will be deformed? Can not use it? Do not open? Is the best professional answer more
A soaked water is not deformed, do not control it, more ventilation or air conditioning dehumidification function, three or five days to dry. The

1. Manufacturer Overview

Location
Year Established
Annual Output Value
Main Markets
Company Certifications

2. Manufacturer Certificates

a) Certification Name  
Range  
Reference  
Validity Period  

3. Manufacturer Capability

a)Trade Capacity  
Nearest Port
Export Percentage
No.of Employees in Trade Department
Language Spoken:
b)Factory Information  
Factory Size:
No. of Production Lines
Contract Manufacturing
Product Price Range

Send your message to us

This is not what you are looking for? Post Buying Request

Similar products

New products

Hot products


Hot Searches

Related keywords