• Aluminum Titanium Boron/AlTi5B1 Coils/AlTi5B1 Rods/Bars System 1
  • Aluminum Titanium Boron/AlTi5B1 Coils/AlTi5B1 Rods/Bars System 2
  • Aluminum Titanium Boron/AlTi5B1 Coils/AlTi5B1 Rods/Bars System 3
Aluminum Titanium Boron/AlTi5B1 Coils/AlTi5B1 Rods/Bars

Aluminum Titanium Boron/AlTi5B1 Coils/AlTi5B1 Rods/Bars

Ref Price:
get latest price
Loading Port:
Tianjin
Payment Terms:
TT OR LC
Min Order Qty:
10 m.t.
Supply Capability:
8000 m.t./month

Add to My Favorites

Follow us:


OKorder Service Pledge

Quality Product, Order Online Tracking, Timely Delivery

OKorder Financial Service

Credit Rating, Credit Services, Credit Purchasing

1.AlTi5B1 Aluminium alloy Introduction:

 .Aluminium titanium boron alloy mainly used for aluminium and aluminium alloy grain refining., improve performance and surface

Quality, add conveniently,  little amount can make excellent effect, universally available in aluminium casting, aluminium profile, aluminium cable, aluminium foils.

.AITi5B1 wire grain refiner produce strong refining results to aluminium and its alloy and with a remarkable effect. Leading to even cast ingot organization, reducing segregation, eliminating Planktonic feather crystal, flaw, and make it reach first- degree grain size.


2.Chemical Composition

Alloy

Composition (%)

Ti

B

Fe

Si

V

impurities

Balance

Form

AlTi5B1    AlTiB5/1

4.5-5.5

0.9-1.1

0.30

0.20

0.20

0.10

Al

Coil, rod, piglet

AlTi3B1    AlTiB3/1

2.8-3.4

0.9-1.1

0.30

0.20

0.10

0.10

Al

Coil, rod, piglet

AlTi5B0.2   AlTiB5/0.2

4.5-5.5

0.15-0.25

0.20

0.30

0.25

0.10

Al

Coil, rod, piglet

AlTi5B0.6   AlTiB5/0.6

4.5-5.5

0.5-0.7

0.30

0.20

0.20

0.10

Al

Coil, rod, piglet


3.Physical Specification

All products are checked by eddy flow while producing, each coil complies with:

Size and Quantity

180kg ±10kg

Inner diameter(mm)

360±25

Outer diameter(mm)

710

Breadth(mm)

280±25

Weight(kg)

180±20

 

4.Grain Refining

AlTi5B1 must be in accordance with the following extreme limit:

Average grain(µ)

Thesumsettle

The highest

Time

AlTi5B1

250µ

400µ

2min.

AlTi3B1

300µ

450µ

2min.

AlTi5B0.6

350µ

500µ

2min.

AlTi5B0.2

450µ

600µ

2min.

 

5.Pictures

Aluminum Titanium Boron/AlTi5B1 Coils/AlTi5B1 Rods/Bars

Aluminum Titanium Boron/AlTi5B1 Coils/AlTi5B1 Rods/Bars


5.FAQ

We have organized several common questions for our clientsmay help you sincerely 

①How about your company

A world class manufacturer & supplier of castings forging in carbon steel and alloy steelis one of the large-scale professional investment casting production bases in China,consisting of both casting foundry forging and machining factory. Annually more than 8000 tons Precision casting and forging parts are exported to markets in Europe,America and Japan. OEM casting and forging service available according to customer’s requirement.

②How to guarantee the quality of the products

We have established the international advanced quality management systemevery link from raw material to final product we have strict quality testWe resolutely put an end to unqualified products flowing into the market. At the same time, we will provide necessary follow-up service assurance.

③How long can we receive the product after purchase?

In the purchase of product within three working days, We will arrange the factory delivery as soon as possible. The pecific time of receiving is related to the state and position of customers.Commonly 7 to 10 working days can be served.

 


Q:Why aluminum wire immersed in copper sulfate solution, static?
Observed phenomenon: the aluminum filament appears purple red solid, the aluminum filament becomes smaller gradually, the solution gradually turns from blue to colorless
Q:Can aluminum wire and copper wire be used instead of tin wire and welded by electric iron?
No, because copper and aluminum have a high melting point, they are generally not melted. Electric irons cannot be melted at all. So instead of seeking acceptance, thank you
Q:What's the side effect of washing aluminum wire basin with detergent?!
Iron and oxygen reaction under room temperature, iron dry air is difficult to react with oxygen. In the humid air, iron and oxygen slow oxidation generated rust (main component: Fe2O3; red rust, loose structure, easy to absorb water, accelerate the corrosion of iron and iron); after a slow oxidation after formation the compounds can also be considered in pure iron oxide, 4Fe+3O2=Fe2O3., wire can be ignited, combustion, Mars radiance, generating solid black, release a lot of heat (in the light before the first wire grinding, in the set of cylinders have a small amount of fine sand or water, to prevent the high temperature spatters burst bottom): 3Fe+2O2 - Fe3O4. light from the above experiment phenomenon, can be seen: "the same material under different reaction conditions, the phenomenon may be different, product may be different"
Q:The air outlet of an aluminum screw into Skoda crystal sharp front windshield!
Fell into the outlet no more major events, it will not only have much impression on the car, take it expensive, several hundred, with no matter what is best not to split the table, and a big gap back to the table table,,
Q:With a broken rod can pine, or drill drilling with curved hair?
Don't change the basin immediately after you take the bend. Die was heard, a middle branch xylem of my pinusthunbergii digging light not only bark alive.
Q:What type of cable should be used for direct buried lighting cables?
Armoured all plastic copper core cable, that is, plastic insulation or sheath, is covered with armor outside it, used to fight against possible mechanical external forces, plays a protective role on the cable.
Q:When fuse is blown, why not use copper wire and wire instead?
Copper wire, aluminum wire, wire resistance is very low, small series power, it is not easy to heat, especially the high melting point of these materials, it is not easy to fuse
Q:What is aluminum magnesium alloy aluminum wire?
Hard aluminium magnesium alloy aluminum lightweight, low density, good heat dissipation, strong resistance, can fully meet the needs of the 3C products are highly integrated, lightweight, miniaturization, anti-collision and electromagnetic shielding and thermal requirements. Its hardness is several times more than traditional plastic chassis, but the weight is only 1/3 of the latter
Q:Home wire is a copper wire, one is aluminum wire, what are the effects and consequences?
Talent ah, such a method for you to think out, using copper wire to do FireWire, aluminum wire to do zero line
Q:How to bind overhead wires?
A wire is a component used to conduct electricity and to transmit electrical energy. Overhead bare wire is usually one phase, 220kV and above line, because of the large transmission capacity, at the same time, in order to reduce corona losses and corona interference, the use of phase split wire, that is, each phase using two or more wires. The split conductor can deliver larger electric energy, and it has less power consumption and better anti vibration performance. The conductor is often tested by various natural conditions in operation. It must have the characteristics of good conductivity, high mechanical strength, light quality, low price, strong corrosion resistance and so on. As China's aluminum resources than copper rich, coupled with aluminum and copper prices vary greatly, so almost all use steel cored aluminum stranded wire.

1. Manufacturer Overview

Location
Year Established
Annual Output Value
Main Markets
Company Certifications

2. Manufacturer Certificates

a) Certification Name  
Range  
Reference  
Validity Period  

3. Manufacturer Capability

a)Trade Capacity  
Nearest Port
Export Percentage
No.of Employees in Trade Department
Language Spoken:
b)Factory Information  
Factory Size:
No. of Production Lines
Contract Manufacturing
Product Price Range

Send your message to us

This is not what you are looking for? Post Buying Request

Similar products

New products

Hot products


Hot Searches

Related keywords