• Met    Coke   of    CSR   64 System 1
  • Met    Coke   of    CSR   64 System 2
  • Met    Coke   of    CSR   64 System 3
  • Met    Coke   of    CSR   64 System 4
Met    Coke   of    CSR   64

Met Coke of CSR 64

Ref Price:
get latest price
Loading Port:
Tianjin
Payment Terms:
TT OR LC
Min Order Qty:
100 m.t.
Supply Capability:
3000 m.t./month

Add to My Favorites

Follow us:


OKorder Service Pledge

Quality Product, Order Online Tracking, Timely Delivery

OKorder Financial Service

Credit Rating, Credit Services, Credit Purchasing

1. Structure of Met    Coke   of    CSR   64   Description

Coke is a hard texture, with carbon as the main component of irregular porous body, with cracks and defects in silver. The true density is 1.8 ~ 1.95 g/cm3, bulk density is 400 ~ 500 kg/m3, the porosity of 35% ~ 35%,.Coke all vertical and horizontal crack can be seen with the naked eye observation. The vertical and horizontal crack along the thick break, still is focal piece containing micro cracks.

Coke production of coking coal (coking coal), also known as metallurgical coal, belongs to the bituminous coal or sub-bituminous coal. Or use the various ratio of coal blend coking. Coking coal in the coke oven is isolated from oxygen after 1000 ° C carbonization is volatile component has been removing, the rest of the solid matter or coke. With the need of ironmaking as little as possible of sulphur, phosphorus pests, so should choose low sulfur, low phosphorus of coking coal.

2. Main Features of the Met    Coke   of    CSR   64

     Quality assurance

     Mutual benefit

     Preferential price

     Various choice

3. Met    Coke   of    CSR   64 Images:

 

Met    Coke   of    CSR   64

Met    Coke   of    CSR   64

Met    Coke   of    CSR   64

Met    Coke   of    CSR   64


4. Met    Coke   of    CSR   64 Specification:

 

Parameters

Guarantee

Moisture (ARB)

5% max

Ash (DB)

12.50% max

Volatile Matter  (DB)

1.4% max

Sulphur (DB)

0.7% max

Phosphorus (DB)

0.035% max

CSR

64% min

CRI

28% max

M40

82% min

M10

8% max

Size 30-90 mm –  90% min

ON SQUARE MESH SCREEN

+90 mm

5% max

-30mm

5% max

Mean Size

52 mm


5. FAQ

We have organized several common questions for our clients,may help you sincerely:

1) Main type

Metallurgical coke is blast furnace coke, coke, iron alloy and nonferrous metal smelting with coke. As more than 90% of the metallurgical coke for blast furnace ironmaking, so often called the blast furnace coke metallurgical coke.

Foundry coke is dedicated to cupola molten iron. Coke is the main fuel of cupola molten iron. Its role is hot metal melting furnace charge and overheating, support stock column maintain its good air permeability. As a result, coke blocks should have large, low reactivity, low porosity, with sufficient impact crushing strength, ash content and low sulfur content.

2) Application of coke

     Used for blast furnace ironmaking and used for copper, lead, zinc, titanium, antimony, mercury

     Other non-ferrous metal smelting of blast furnace,

     Reducing agent, compound

     The function of stock column frame.

3) The history of coke

From around the world, the coking coal resources are scarce, it is the precious resources must be protected, so has been seldom used coking coal coking alone. In China, the first kind of typical coal coking coal with hebei feng feng coal mine, shanxi gujiao cetrimonium, heilongjiang drops of jixi, anhui huaibei zhangzhuang and dabao top-coal panzhihua in sichuan province.The second category of typical coal coking coal have jilin tonghua iron works and the Inner Mongolia baotou beach ditch coal.Benxi, northeast China hebei tangshan, jingxing, shandong xinwen, etc., are all famous origin of coking coal.



Q:After the long-term use of non stick pan, oil stains can not be effectively removed, over a long period of time in the non stick coating on the formation of a layer of coke, the effect of losing non stick. As a result of this layer of coke is relatively dense and smooth, scouring cloth has been ineffective, steel ball can not be used to damage the coating, what chemical or physical methods to remove this layer of coke?
Four, wash the metal wire ball friction force discoloration, and always use water to clean out the dirt.So that the whole place to restore the original black dye can be done.Water sandpaper rubbing can of course, but in the end to more than 1000 mesh water sandpapering. Another 100 clean cloth polishing line. The coke on the stove can only be removed by hand.Finally, wash the rice cooker, stove, as well as your tired hands, thoroughly washed several times. Here, everything is back to normal, as if nothing had happened.
Q:What is the difference between coking plant and coke plant
Production equipment and production processes are complex.Coke plant, generally only the coal into coke on it, so simple.
Q:Coke is divided into several kinds of specifications ah
Three: 1 2 3 coke metallurgical coke of high sulfur cokeCoke is in coal under the condition of air isolation, heating to 950-1050 DEG C, after drying, pyrolysis, melting, bonding, curing and contraction of the final stage is made, the process is called high temperature coking (high temperature carbonization). Coke obtained from high temperature coking for blast furnace smelting, casting and gasification. Coke oven gas produced in the process of coking and recovery is not only a high calorific value of fuel, but also an important industrial raw material for organic synthesis. Coke is mainly used in blast furnace ironmaking and smelting of non-ferrous metals such as copper, lead, zinc, titanium, antimony, mercury and so on.
Q:What is the reasonable ratio of coal to coke
There are lignite, bituminous coal, anthracite, semi anthracite these categories. Under the condition of isolated air, the bituminous coal is heated to 950-1050 DEG C, and finally, the coke is made by drying, pyrolysis, melting, bonding, solidification and shrinkage.
Q:Standard grade two grade coke standard
5, the moisture in the coke: water fluctuations will make the measurement of coke is not allowed, resulting in fluctuations in furnace conditions. In addition, the increase in the moisture content of Coke will make the M04 high, M10 is low, the drum index error.6, the screening of coke composition: in the blast furnace coke particle size is also very important. In the past, the particle size of coke in our country is as follows: the coke size of large coke oven (1300 - 2000 square meters) is greater than 40 mm; the coke size of medium and small blast furnace is larger than 25 mm. However, some of the steel test shows that the coke particle size of 40 - 25 mm as well. Larger than 80 mm of coke to be whole, so that the particle size range. The coke block is uniform, the gap is large, the resistance is small, and the furnace condition runs well.
Q:What are the criteria for coke classification and how to distinguish between primary and two grade coke?
Quality index of cokeCoke is the solid product of high temperature carbonization, the main ingredient is carbon, is the pore structure has a crack and irregular (or pore porous). The crack number directly affects the coke strength and crushing strength, the index generally refers to the unit volume of the crack (crack number within the coke grain length). To measure the pore structure of the main indicators to measure with porosity (only coke pore volume accounted for percentage of the total volume) that it affects the coke reactivity and strength. The different uses of the coke porosity index for different requirements, the general metallurgical coke gas hole rate in 40 ~ 45%, foundry requirements in 35 ~ 40%, coke export requirements in 30%. Coke crack degree and the porosity level, and the coking coal has a direct relationship, such as coal based coke refining, crack, high porosity, low strength and coking coal as a base; Coke coal refining. Crack less, low porosity and high strength. The strength of coke is used to denote the crushing strength and abrasion resistance of two indicators. The coke crushing strength is that coke can resist foreign impact force without ability along cracks or defects at the broken table, shown by M40 wear; strength of coke coke refers to the ability to resist external friction without surface of glass forming debris or powder, by the M10 value. The effect of the crack of coke crushing strength, M40 value, M10 value and abrasion strength influence of coke pore structure. M40 and M10 were determined by lot. In China the migon drum test in Germany.
Q:China's coke iron smelting began in what time?
Han also invented the "fried steel law", that is, the use of pig iron "fried" mature iron or steel of the new process, the product is called steel. At the same time, the rise of "100 steelmaking" technology. The Eastern Han Dynasty (AD 25 ~ 220), when the emperor of the Ming Dynasty, invented the hydraulic blast furnace, that is, "water discharge". The invention of ancient water row in China, about 1100 years earlier than europe. After the Han Dynasty, the method of steel. "Qi Shu Qi, even referred to as" places "big steel", later known as the filling steel, also known as steel group. This is another important achievement of the ancient steelmaking technology in china. According to the "Encyclopedia of" records: Chinese is the earliest use of coal iron country, the Han Dynasty have been tried, song and Yuan dynasties have been popularized. To the Ming Dynasty (AD 1368 ~ 1644) has been able to use coke smelting pig iron.
Q:Who knows the proportion of pig iron and coke used in Cupola
There are doubts: if the scrap ratio is too large to increase the difficulty of processing, product quality can not be guaranteed. The proportion is too high or too low are abnormal.2, auxiliary material input: foundry auxiliary materials mainly coke. Ordinary casting (except dry cylinder) 1 tons ~ ~ 5 tons cupola, each investment of 1 tons of coke, according to the situation of the piece can be from 4.5 tons to 5.5 tons. Ordinary blank (special pieces extra), 5 tons to 10 tons per 1 tons of coke in cupola furnace about 6.5 tons to 7.5 tons of blank (waste products re melted are calculated according to the above method).
Q:Coke is how to make it? What is the use?
Improving the coal preparation process is the way to expand the coking coal source and improve the quality of coke. At present, most of the coking plants in China adopt the mixed grinding process. This process can not be treated according to the different hardness of coal, so it is only suitable for the coking coal with good caking property and uniform coal quality. A new coal preparation process has three kinds: single comminution process is various, coal crushing alone first, and then according to the provisions of the proportion, then mixing; the first group grinding process, hardness of similar kinds of coal, according to the proportion of each group, were sent to the respective crushing requirements the particle size, then mixing the crushing process; is crushed to a certain degree of coal sieving, the coarse grain group screened were crushed again, so that the coarse grain group cohesiveness, inert material with high content of ground fine, avoid good bonding facies excessive grinding components.
Q:Why is coke used in blast furnace steelmaking?Why not use coal?
(2) reduction: high temperature gas generated in coke combustion in the raceway, passed to the material in the process of heat rising, the endothermic reaction and coke formation, CO and H2, then CO and iron oxide in iron ore reduction reaction is transformed into metallic iron.(3) the role of the skeleton: the blast furnace smelting process occurs in the movement and interaction between the rising of the gas and the falling of the charge. The pellets, coke, iron ore, ore and other materials according to a certain proportion, and batch sequence into a blast furnace, blast furnace smelting in reducing atmosphere under the hot metal, after providing to the steelmaking plant of the steel-making.

1. Manufacturer Overview

Location
Year Established
Annual Output Value
Main Markets
Company Certifications

2. Manufacturer Certificates

a) Certification Name  
Range  
Reference  
Validity Period  

3. Manufacturer Capability

a)Trade Capacity  
Nearest Port
Export Percentage
No.of Employees in Trade Department
Language Spoken:
b)Factory Information  
Factory Size:
No. of Production Lines
Contract Manufacturing
Product Price Range

Send your message to us

This is not what you are looking for? Post Buying Request

Similar products

New products

Hot products