What's the hardness of 7075 aluminum bars?
Tensile strength 524Mpa:0.2%Yield strength 455Mpa: elongation 11%Modulus of elasticity E/Gpa:71Hardness: 150HBDensity: 2850
30mm aluminum rod with CNC lathe cutting what blade? How much speed? Feed?
With NC3020 blade, 3 mm wide. Speed 1500-2000, feed speed F0.1-0.15 mm / turn, can also be suitable to improve the line. Answer satisfaction, please adopt and give high praise. Thank you
What can make the aluminum bar surface shiny?
2, the formation of aluminum hydroxide3, aluminum hydroxide heating decompositionCase 2: low concentration dilute hydrochloric acid solution (HCL)1. Dip the alumina into dilute hydrochloric acid of low concentration2, after a period of three, remove two aluminum oxide
1060 pure aluminum rods, how to process hardness?
Aluminum sword, if you chop it at high speed, it can also kill effect. Piercing can be hurt.
Their own factories need to invest much money
Smelting aluminum ingot, aluminum rod pollution, high cost. What's the market like?
nan
If 2000 can not be conveyed, the line speed is only about 50 meters;
Is pure aluminum not the raw material? Why are pure aluminum rods hollow? Time consuming and exhausting. Who can introduce?!!! Thank you!! (the country has banned the export tax refund of pure aluminum products). Why is the product still exported to Korea and Japan?.
As to why pure aluminum rods are made of hollow, this is an industrial consideration, and I do not know......
How to deal with the burning of 6061 aluminum bars in hard oxidation?
This is because the anodic oxidation process can not effectively heat dissipation, resulting in severe overheating. At first, the burning is localized.