General information of low carbon wood
Raw material |
Sawdust, corn-straw and tailing, can be recycled after using. |
Technology |
Utilizing molecular structure of crystalline-state solidification, shaping under normal temperature and pressure with low carbon emission. |
Installation |
Stitching, wet-sticking and dry-fasten connecting |
Character |
Favorable corrosion resistance, non-ignitable, water-proof, UV-resistant, high resistance to fire, water and insects. |
Lead time |
30 days after receiving buyer's original L/C or Prepayment |
Package |
Seaworthy Export Standard Wooden Pallet |
Four breakthroughs |
Comprehensive utilization of natural resources: Be recyclable, using sawdust, corn-straw and tailing as materials. The product can be recycled after using. |
Low carbon and energy saving in the course of production: Adopting the independent individual property’s technology, utilizing molecular structure of crystalline-state solidification, shaping under normal temperature and pressure with low carbon emission. | |
Environmental and healthy in the course of construction and using: Synthesized by natural inorganic raw materials, nontoxic, odorless and non-radiative simple installation, which could save energy cost and reduce and waste emission, raise efficiency and reduce erection time. | |
From nature, beyond nature: Full realization of the natural texture, high resistance to fire, water and insects. Do not rot or fade after long time usage. Super self-cleaning needs low maintenance cost. Vivid color and appearance provides a wide space to designers. | |
Six advantages |
Lower more than 50% cost, enhance building's performance to price ratio. |
Cutting at will, Fixing easy, Shorting project time. | |
Good performance in resistance to elements, corrosion-resistant ,resistance to termite, fire resistance and water-resistant, far from distortion and discolorations in 30 years. | |
Well self-cleaning, low cost in later maintenance: Don't need professional maintenance in 30s(Cleaning with water only), saving much cost. | |
Customize the color, showing individuation: Beyond 400 kinds of colors, designers could exhibit their imagination. | |
Compound with natural inorganic materials: Without formaldehyde and toluol, sustained releasing negative oxygen ion, forming nature oxygen bar. | |
Special specifications are available on customers' requirements. |
Specification of low carbon wood
Standard: 3000mm(L)×1200mm(W)×15mm(T)
Standard length: 3000mm
Standard width: 120mm,150mm,200mm,300mm(including 3mm kerf width)
Standard thickness: 15mm
Technical information of low carbon wood
Density |
1.26g/m3 |
Folding strength |
10Mpa |
Dry-shrinkage rate |
0.05% |
Elastic modulus |
7211Mpa |
Wet expansion rate |
0.17% |
Shear strength |
3.5Mpa |
Screw holding capability |
121N/mm |
Coefficient of heat conductivity |
0.69(W(m·k)) |
Frost resistance |
Thaw-freeze cycle after 30 times, no slip crack and peeling off | ||
Unpermeability |
No drop appearing on the bottom after 24 hours. | ||
Impact strength |
3.3KJ/m2 |
Products exhibition of low carbon wood
Low carbon wood sheets with thin grain
Low carbon wood sheets with thick grain
The project picture of low carbon wood
- Q: Veneer production process is this?
- The most effective way to improve the plasticity of wood is to adjust both the temperature and the moisture content at the same time to increase the temperature of the wood while increasing the moisture content of the wood
- Q: Simple construction method of veneer
- Veneer is due to a large number of wood cutting in recent years, and the slow growth of logs
- Q: How to seize the key to solve the problem of slow development of paste veneer process?
- According to professional survey found that upgrading the veneer process not only to ensure the quality of veneer and production level, but also need a suitable veneer glue
- Q: The Veneer dyeing quality requirements
- The next step to deal with, and then after a good modulation of the pigment (dye) soaked, the basic veneer has a color, and then fixed color, drying, hot pressing, cutting, packaging.
- Q: Slicing of thin slices of wood
- after cooking treatment; the cooking process should be reduced to more than 40 ℃, it should slow down the heating rate
- Q: Technology veneer and natural veneer distinction
- This is the case all over the world. This is not to say. All understand. Technology veneer although there is no natural veneer texture naturally nice.
- Q: Part of the production process
- After the wood side has been cooked (ie, water heat treatment), the plasticity of the wood increases
- Q: Different veneer has different production processes
- Most furniture companies believe that science and technology veneer is not a native wood, but what is it, they also do not know, or simply called "artificial veneer".
- Q: What is the size of the veneer?
- Simple veneer operation, will be applied to the veneer of the wood surface treatment is clean, there are rugged to be dealt with first flat
- Q: The Sliced ??veneer manufacturing process
- Wood → truncated → cut → softened (steamed or boiled) → slicing → drying (or not drying) → cutting → inspection packaging → storage
Send your message to us
High Quality Low Carbon Wood Veneers Sheets 001
- Loading Port:
- China Main Port
- Payment Terms:
- TT or L/C
- Min Order Qty:
- 1000 sq.m, m²
- Supply Capability:
- 400000 sq.m. Per Month m²/month
OKorder Service Pledge
OKorder Financial Service
Similar products
Hot products
Hot Searches