General information of low carbon wood
Raw material |
Sawdust, corn-straw and tailing, can be recycled after using. |
Technology |
Utilizing molecular structure of crystalline-state solidification, shaping under normal temperature and pressure with low carbon emission. |
Installation |
Stitching, wet-sticking and dry-fasten connecting |
Character |
Favorable corrosion resistance, non-ignitable, water-proof, UV-resistant, high resistance to fire, water and insects. |
Lead time |
30 days after receiving buyer's original L/C or Prepayment |
Package |
Seaworthy Export Standard Wooden Pallet |
Four breakthroughs |
Comprehensive utilization of natural resources: Be recyclable, using sawdust, corn-straw and tailing as materials. The product can be recycled after using. |
Low carbon and energy saving in the course of production: Adopting the independent individual property’s technology, utilizing molecular structure of crystalline-state solidification, shaping under normal temperature and pressure with low carbon emission. | |
Environmental and healthy in the course of construction and using: Synthesized by natural inorganic raw materials, nontoxic, odorless and non-radiative simple installation, which could save energy cost and reduce and waste emission, raise efficiency and reduce erection time. | |
From nature, beyond nature: Full realization of the natural texture, high resistance to fire, water and insects. Do not rot or fade after long time usage. Super self-cleaning needs low maintenance cost. Vivid color and appearance provides a wide space to designers. | |
Six advantages |
Lower more than 50% cost, enhance building's performance to price ratio. |
Cutting at will, Fixing easy, Shorting project time. | |
Good performance in resistance to elements, corrosion-resistant ,resistance to termite, fire resistance and water-resistant, far from distortion and discolorations in 30 years. | |
Well self-cleaning, low cost in later maintenance: Don't need professional maintenance in 30s(Cleaning with water only), saving much cost. | |
Customize the color, showing individuation: Beyond 400 kinds of colors, designers could exhibit their imagination. | |
Compound with natural inorganic materials: Without formaldehyde and toluol, sustained releasing negative oxygen ion, forming nature oxygen bar. | |
Special specifications are available on customers' requirements. |
Specification of low carbon wood
Standard: 3000mm(L)×1200mm(W)×15mm(T)
Standard length: 3000mm
Standard width: 120mm,150mm,200mm,300mm(including 3mm kerf width)
Standard thickness: 15mm
Technical information of low carbon wood
Density |
1.26g/m3 |
Folding strength |
10Mpa |
Dry-shrinkage rate |
0.05% |
Elastic modulus |
7211Mpa |
Wet expansion rate |
0.17% |
Shear strength |
3.5Mpa |
Screw holding capability |
121N/mm |
Coefficient of heat conductivity |
0.69(W(m·k)) |
Frost resistance |
Thaw-freeze cycle after 30 times, no slip crack and peeling off | ||
Unpermeability |
No drop appearing on the bottom after 24 hours. | ||
Impact strength |
3.3KJ/m2 |
Products exhibition of low carbon wood
Low carbon wood sheets with thin grain
Low carbon wood sheets with thick grain
Project picture of low carbon wood
- Q: Veneer production process is this?
- This is the actual production is usually used saturated steam or hot water on the wood side of the cooking treatment of a water heat treatment reasons
- Q: How to seize the key to solve the problem of slow development of paste veneer process?
- Under normal circumstances, the designer is the use of Wan Nengjiao and white latex, and these two kinds of glue has a great flaw
- Q: Cut Slicing - The cut is a round of vertical cut logs, producing a veneer with a ruled ridge.
- Lengthwise Slicing - Cut the flat saws flat through the fixed slicer and cut the veneer from the bottom of the plate. The texture of the longitudinal cut veneer is varied.
- Q: Technology veneer and natural veneer distinction
- This is the case all over the world. This is not to say. All understand. Technology veneer although there is no natural veneer texture naturally nice.
- Q: Wooden door with veneer ruled, pattern is produced by different cutting methods
- cut out the wood. From the cut off the logs cut off the veneer, the first layer of the ring will form a "cathedral" type of pattern grain.
- Q: Different veneer has different production processes
- Most furniture companies believe that science and technology veneer is not a native wood, but what is it, they also do not know, or simply called "artificial veneer".
- Q: What is the veneer panel
- Veneer panel commonly known as panel. Is the solid wood board precision cut into a thickness of about 0.2mm meager veneer for the surface layer to the splint as the substrate,
- Q: Veneer should pay attention to the different production processes
- But the technology veneer is widely recognized by the furniture industry still need time, science and technology on the wood of many misunderstandings, are the lack of factual basis, is the understanding of the errors.
- Q: Different cutting processes of wood veneer
- Finally, the term "technology veneer" can not accurately express the essence of the product, and it is easy to misunderstand. In foreign countries, "technology wood" is generally referred to as "landscaping", "reorganized wood" or "combination Wood "
- Q: The Sliced ??veneer manufacturing process
- After the logs are put into the factory, the cuttings must first be cut in accordance with the required length,
Send your message to us
High Quality Low Carbon Oak Wood Veneers 003
- Loading Port:
- China Main Port
- Payment Terms:
- TT or L/C
- Min Order Qty:
- 1000 sq.m, m²
- Supply Capability:
- 400000 sq.m. Per Month m²/month
OKorder Service Pledge
OKorder Financial Service
Similar products
Hot products
Hot Searches