AISI, ASTM, BS, DIN, GB, JIS Phosphatized Steel Wire
- Loading Port:
- Tianjin
- Payment Terms:
- TT OR LC
- Min Order Qty:
- 50 m.t.
- Supply Capability:
- 10000 m.t./month
OKorder Service Pledge
Quality Product, Order Online Tracking, Timely Delivery
OKorder Financial Service
Credit Rating, Credit Services, Credit Purchasing
You Might Also Like
Quick Details
Steel Grade: 65# 70# 72A
Standard: AISI, ASTM, BS, DIN, GB, JIS
Wire Gauge: 0.43-3mm
- Type: Phosphatized
Application: Hold up
Alloy Or Not: Is Alloy
Special Use: Free Cutting Steel
- Phosphatized: Bright
Packaging & Delivery
Packaging Details: | Paper Cores or bundles or as customer's requirements |
---|---|
Delivery Detail: | 7 days after receving the 30% advanced payment |
Specifications
Diameter:0.43-3mm
Tensile strength:1320-1960
Use:Optical Cable for holding up
It is a top-qulity product of Hebei Province which is used for holding up for the optical cable.
Phosphatized Steel Wire | |
Dia. (mm) | Tensile Strength(Mpa) |
0.43≤d≤0.60 | 1960 |
0.60≤d≤0.80 | 1770 |
0.80≤d≤1.10 | 1670 |
1.10≤d≤1.90 | 1570 |
1.90≤d≤2.50 | 1470 |
2.50≤d≤3.00 | 1320 |
Phosphatized Steel Wire | |||||||
Dia. | Sample Length | Torsions (times) | |||||
Tensile Strength(Mpa) | |||||||
mm | 1320 | 1470 | 1570 | 1670 | 1770 | 1960 | |
0.50≤d≤1.00 | 100*d | - | - | - | 28 | 27 | 24 |
1.00≤d≤1.30 | - | - | 28 | 27 | - | - | |
1.30≤d≤1.80 | - | - | 27 | - | - | - | |
1.80≤d≤2.30 | - | 25 | 25 | - | - | - | |
2.30≤d≤3.30 | 24 | 23 | - | - | - | - |
Phosphatized Steel Wire | |
Dia. (mm) | Tolerance (mm) |
0.43 | ±0.01 |
0.50 | |
0.60 | |
0.70 | |
0.80 | |
0.90 | ±0.02 |
1.00 | |
1.10 | |
1.20 | |
1.30 | |
1.40 | |
1.50 | |
1.60 | ±0.03 |
1.70 | |
1.80 | |
1.90 | |
2.00 | |
2.10 | |
2.20 | |
2.30 | |
2.40 | |
2.50 | |
2.60 | |
2.70 | |
2.80 | |
2.90 | |
3.00 |
Phosphatized Steel Wire | |||||||
Dia. | Circle of bending raduis | Bends (times) | |||||
Tensile Strength(Mpa) | |||||||
mm | 1320 | 1470 | 1570 | 1670 | 1770 | 1960 | |
0.50 | 1.25 | - | - | - | - | - | 5 |
0.60 | 1.75 | - | - | - | - | - | 9 |
0.70 | - | - | - | - | 7 | - | |
0.80 | 2.50 | - | - | - | - | 13 | - |
0.90 | - | - | - | 11 | - | - | |
1.00 | - | - | - | 9 | - | - | |
1.10 | Right 3.75 | - | - | - | 16 | - | - |
1.20 | - | - | 15 | - | - | - | |
1.30 | - | - | 13 | - | - | - | |
1.40 | - | - | 11 | - | - | - | |
1.50 | - | - | 10 | - | - | - | |
1.60 | 5.0 | - | - | 13 | - | - | - |
1.70 | - | - | 12 | - | - | - | |
1.80 | - | - | 11 | - | - | - | |
1.90 | - | - | 10 | - | - | - | |
2.00 | - | 10 | - | - | - | - | |
2.10 | 7.5 | - | 14 | - | - | - | - |
2.20 | - | 13 | - | - | - | - | |
2.30 | - | 12 | - | - | - | - | |
2.40 | - | 11 | - | - | - | - | |
2.50 | - | 10 | - | - | - | - | |
2.60 | 10 | - | - | - | - | - | |
2.70 | 9 | - | - | - | - | - | |
2.80 | 9 | - | - | - | - | - | |
2.90 | 8 | - | - | - | - | - | |
3.00 | 8 | - | - | - | - | - |
- Q: Why can't aluminum and other metals be heated in an electromagnetic oven?
- There are mainly two parts in the induction cooker: the electronic circuit and the structural package.The electronic circuit parts include power board, main board, lamp board, coil plate and heat sensitive bracket, fan motor and so on.The structural part of the packaging include: porcelain, plastic cover, fan blade, fan bracket, power line, power operation manual, stickers, film, certificate, plastic bags, foam, shockproof box, bar code, cartoon box.According to the principle of operation, iron cookers must be used.
- Q: Will the metal ions in the layered composite metal oxides be replaced by other ions?
- Are generally ionic compounds, namely active metal loses electrons form positively charged cations, and non metal electronic form negatively charged anions, cations and anions by electrostatic interaction to form ionic compounds.
- Q: Can we import scrap tanks and other scrap metals from Russia?
- Imports of scrap metals, as long as there is no safety problems (radiation, biological safety, etc.), can be from any country, of course, the premise is the cost of the economy. Because the current domestic steel overcapacity, iron and steel prices can not be lower, and even some steel prices lower than the cost price (major steel mills low price struggle against the vicious results of the market). So be sure not to import more than new domestic steel.
- Q: What is the sign of PD? What are the signs of other precious metals?
- Platinum (Pt) - acid ferric chloride at room temperature. But it can be slow, aqua corrosion, hydrochloric acid only adding oxidant to the corrosion of platinum, platinum in hydrobromic acid corrosion at room temperature under high temperature corrosion can platinum halogen, molten potassium (sodium) to platinum platinum dissolved in strong corrosion. Boiling aqua regia and sulfuric acid.Platinum (PD) attracts organic vapors. Carbon and carbide affect physical and mechanical properties, so contact with this material should be avoided in the manufacture and use of platinum palladium and its alloys
- Q: What metal has the fastest heating?
- In daily life, copper burns fastest.The effect of thermal dispersion is related to thermal conductivity. The greater the thermal conductivity, the better the effect of heat dissipation.
- Q: Is the acquisition of scrap metals controlled by the police? Any other takeover of the police?
- The production of scrap metal business, shall be approved by the competent department for examination of their consent to the local people's government at the county level public security organs for the issuance of special trade license, and apply for registration to the administrative department for Industry and commerce at the same level, receive special trade license and business license, shall be allowed to open.
- Q: What does "active metal" mean?
- Determination of metal is lively and can replace metal hydride in hydrogen, the hydrogen by replacement reaction to elemental hydrogen, if the hydrogen in metal hydride elements that determine the first replacement out of the metal active, then can react with metal hydride to determine the strength of the order of the number of active metal
- Q: Are iron and steel nonferrous metals?
- The broad range of nonferrous metals also includes nonferrous alloys. A nonferrous alloy is an alloy consisting of one or more other elements with a base (usually greater than 50%) of a nonferrous metal.
- Q: What does "productive scrap metal recycling" mean?
- Productive scrap metal recycling refers to the recycling of metal materials and metal products used in construction, railways, communications, power, water conservancy, oil fields, national defense and other production areas, and has lost its original use value.
- Q: What metal does nonmagnetic metal have?
- Other than these, most are not ferromagnetic, such as copper, aluminum, magnesium, zinc, and so on
Send your message to us
AISI, ASTM, BS, DIN, GB, JIS Phosphatized Steel Wire
- Loading Port:
- Tianjin
- Payment Terms:
- TT OR LC
- Min Order Qty:
- 50 m.t.
- Supply Capability:
- 10000 m.t./month
OKorder Service Pledge
Quality Product, Order Online Tracking, Timely Delivery
OKorder Financial Service
Credit Rating, Credit Services, Credit Purchasing
Similar products
Hot products
Hot Searches
Related keywords