Product Description:

 Structure of Plastic Sheet Hdpe Geomembrane

Good mechanical properties, high tear strength, deformation and adaptable, puncture resistance, anti-aging, anti-ultraviolet-resistant,

Anti oil and salt, pH, anti-corrosion, high temperature-resistant, non-toxic, long service life. water, drainage, seepage, the good effect of moisture, width, thickness of the full range of specifications and low cost, simple construction.

Main Features of Plastic Sheet Hdpe Geomembrane

 1) thickness : 0.1mm - 4.0mm.

 2) width : Within 8 m (1m-8m).

 3) length : 50-100m/roll (as request).

 4) Material : HDPE,( LDPE, LLDPE, PVC, EVA ,CPE).

 5) Color : Black , white , red , blue , or as required.

Plastic Sheet Hdpe Geomembrane Images

 

Waterproof Polyethylene Geomembrane with Colorful for Pond 

Waterproof Polyethylene Geomembrane with Colorful for Pond

 

Waterproof Polyethylene Geomembrane with Colorful for Pond

Waterproof Polyethylene Geomembrane with Colorful for Pond

Plastic Sheet Hdpe Geomembrane Specification:

 

No.

Item

              Test Value

0.75mm

1.0 mm

1.25 mm

1.5 mm

2.0 mm

2.5 mm

3.0mm

1

Minimum Density(g/cm³)

0.939

2

 

Tensile Property

Strength at yield,N/mm

11

15

18

22

29

37

44

Strength at break ,N/mm

20

27

33

40

53

67

80

Elongation at yield,%

12

Elongation at break,%

700

3

Tear Resistance   N

93

125

156

187

249

311

374

4

Puncture Resistance  N

240

320

400

480

640

800

960

5

Stress Crack Resistance, hrs

300

 6

Carbon Black Content, %

2.0-3.0

Carbon Black Dispersion

1  or  2

 7

Standard OTI  Min

100

High Pressure OTI  Min

400

8

Impact Cold Crack at -70°C 

Pass

9

Water vapor permeability

 (g.cm/cm2 .s.Pa)

≤1.0×10-13

10

Dimensional Stability (%)

±2

 

FAQ:

1. How about the delivery time?    

    Two weeks upon receipt of down payment. 

2. What kind of payments do we accepted?   

   T/T, L/C, WesternUnion, MoneyGram. 

3. What's are the MOQ?   

    Normally the MOQ is 5000 SQM in theory. 

    And we can provide you free samples for quality inspection.  

4. Do you charge for the samples?   

    Accordeing to our company policy, the samples are freee, we only charge the freight fee. And we will return the freight fee in your second order.   

5. Can you produce the product according to customers' requirements?

     Sure, we are professional manufacturer, OEM and ODM are both welcome

 

 

Send a message to us:

Remaining: 4000 characters

- Self introduction

- Required specifications

- Inquire about price/MOQ

Q:Function introduction of geomembrane welding machine
whose role is to weld two geomembranes into one, just like welding two metal plates into one.
Q:How to make sure there is no bubble on the film?
1. Cutting: The specifications of glass film are cut into veneers than are to be larger than about 1cm. This will avoid the trouble of sticking to the side (while more than one side) and repeating again. 2. To clean the glass: Before pasting the glass paper, the grease, stains and dust on the glass should be cleaned with enough water( the best is t o add some liquid detergent). The purpose of spraying water is to temporarily reduce the viscosity of the glass film, and the viscosity of the glass film will not be affected after it is dry. 3. To remove the back release liner: To remove the membrane type glass film back (with rubber surface) also enough spray in the water, it will paste process can random in the glass move back and forth which is convenient to the proper position. 4. Pasting: First, to paste the glass film on the glass after the average proportion, and post it on the glass top and aligned paste from the top to the down. If it is not alined in one-time, it can be repeatedly reopened to paste (the benefits of spraying water) 5. To exhaust bubbles: To use the scraper or IP card from the center to the around water and scraping bubble, catch out water and air bubbles with a needle or blade punctured to smooth. Until there is no any water and air bubbles, and the glass film is completely sticked on the glass so far. 6. To cut off the rest part: After pasting the film, to cut off the excess part with the blade.
Q:which kind of imitation wood film is better?
3M films' price performance is relatively high, but there are also pseudomembranous everywhere. Automotive stick membrane should be considered from the following three aspects: 1, genuine and ahsm of film 2, technology of sticking membrane, 3,after-sales. comprehensively, i advice you order the membrane in large3M authorized stores. about the genuine and sham of membrane, you can consider it from the following three aspects, 1, see the store authorization, the authorization form is authorized one time a year, 2, see the membrane. smell film. the genuine membrane has no peculiar smell. 3, electronic warranty of products. there are lots of pecific construction process, construction specifications, very professional. it's about which kind of film is the best, everyone has their own standard, as each product has it's own focuses, advantages and disadvantages. Each brand includes high-end and low-end products.
Q:What are the specifications of DNP aluminum plastic film?
The specifications of DNP aluminum plastic film: Aluminum plastic plate can be roughly divided into interior decoration board and exterior decoration (curtain wall) board. The specification of aluminum plastic plate used in interior decoration is about 1.22m×2.44m×3mm. The thickness of exterior decoration is about 4mm. The size is not fixed, and they are generally customized.
Q:What is the construction method of the geotechnical membrane?
The construction method: To lay it in the range of measurement. To lay the composite geotechnical membrane before the first required to lay a good sand cushion on the roadbed, laying the width of the design requirements set. When laying, do not allow the laying of folds, as far as possible to tighten. After the pavement, the U type nails or bamboo nails is used to fix. When laying composite geotechnical membrane, the surface of the sand layer is smooth, no hard protrusion, and timely fill sand cover, avoid direct exposure to the sun for a long time. When the composite earthwork film is laid, the length of the transverse lap and the longitudinal lap can meet the design requirements. After the composite geotechnical membrane is rolled out, the filling material is filled up in time, and after the soil is covered with light compaction mechanical compaction, only when the thickness of the overburden layer is larger than 0.6m, the soil can be compacted by heavy compaction machine. Composite geotechnical membrane according to the design requirements can be divided into two types of longitudinal force and lateral force, the laying of composite soil before the film to understand the design intent, strictly according to the design requirements of the laying.
Q:What is the difference between the primer and the basilemma?
The main difference is as follows.Primer is used as back cover. Basilemma can be used as back cover as well as interface agent which can increase the adhesion of sublayer and surface layers.Besides, primer often contains formaldehyde, some of them can even release the formaldehyde (materials containing formaldehyde used on outer wall are not forbidden by national standard). However, quality products of primer are environmental friendly and odorless. So it's better to choose primer as wallpaper.
Q:How to deal with the waterproof membrane on balcony?
1, Cleaning the base; 2, Leveling the base with cement mortar 3, brushing one layer of JS waterproof paint and paving one layer of non-woven fabric immediately. Then brushing a layer of JS waterproof paint again (it should be noted that walls should be flanged up for 300mm); 4, After the waterproof layer is totally dried, you can do the watyer conserving test for 24 hours; 5, After draining the water, you can lay the floor tile on it (it is better to leave the seams with the width of 5mm and brush structural adhesive in it).
Q:How to adhere film to the glass window?
A. Preparatory work and installation of architectural membrane pasting: 1. Preparations before installation a) Learn the specific conditions of the window to be pasted membrane in detail, and estimate specific items for site cleaning, and the size and quantity of the window membrane needed cutting; b) Determine the construction method according to the window membrane type chosen by the customer and characteristics of the the glass; c) Check whether the installation tools are normal, and check if the "blade" of the water wiper is flat and smooth, and if there is any gap existent. Check if the cleaning scraper knife is sharp, and if there is any gap or sawtooth existent; d) Check if the cleaning and installation towel is clean, if the waterproof membrane is clean and intact; e) Prepare the film-on and cleanout fluid well; 2. Installation of window membrane: A. Advance preparations for the construction site. a) In the construction site, remove the curtains, blinds, and all other objects near the window carefully, and make them go back to the original state when the window membrane installation is completed. Try to leave more space for equipment placement. If the construction site is located within an office or store, please make sure that the cleaning work in advance will not interfere with the customer's normal business operations; b) Do a good job in on-site waterproof and cleaning, laying of waterproof membrane, and work overalls and shoe covers wearing;
Q:What are the construction steps of seepage-proof geomembrane?
Quality inspection method of HDPE geomembranes in seepage-proof construction 1: Civil engineering qualified acceptance supporting documents must be issued before paving seepage-proof membranes. 2: Sizes should be accurately measured before cutting the seepage-proof membranes, and then cut in accordance with real sizes, generally it should not be cut according to the icon sizes, and it should be numbered by sheet, and be recorded in detail on special forms. 3: The welding lines should be kept to a minimum range when paving seepage-proof membranes, on the premise of quality assurance, raw materials should be saved. Meanwhile it is easy to ensure the quality. The lapping width of seams between membranes is generally no less than10 cm, the orientation of welding lines is usually parallel to the maximum gradient, namely, arranging along the direction of the gradient. 4: Usually in corners and abnormal sections, the seams should be as short as possible. Apart from special requirements, when the proportion of slope to slope crest is greater than 1:6 or when the stress concentration region is within the 1.5 meters, welding lines should be avoided.
Q:How to stick the film on lampblack machine?
You can just use the preservative film. 1. Pulling the preservative film from its packaging and putting the film on the smoke exhaust hood. Cutting off the film with a blade when the film is stuck to the edge. 2. Pressing and strenghtening the film on the smoke exhaust hood. 3. Sticking the preservative film all over the oil box of the smoke exhaust ventilator. When there is lot of oil, the old film can be repalced by the new one to avoid cleaning the ventilator. Here are some tips. 1. When the preservative film gets dirty, you can just replace it with a new piece. 2. Usually, the film can be changed once a month. 3. In the kitchen, when sticking the film, it is best to pull the film in its package without pulling the membrane core out so that the film can be stuck flat and easily cut off.

1. Manufacturer Overview

Location
Year Established
Annual Output Value
Main Markets
Company Certifications

2. Manufacturer Certificates

a) Certification Name  
Range  
Reference  
Validity Period  

3. Manufacturer Capability

a)Trade Capacity  
Nearest Port
Export Percentage
No.of Employees in Trade Department
Language Spoken:
b)Factory Information  
Factory Size:
No. of Production Lines
Contract Manufacturing
Product Price Range