Product Description:

 

Description Of  EVA,HDPE,LLDPE,PVC,LDPE Material HDPE geomembrane:

Type:HDPE geomembrane
Material: High-density polyethyle
Thickness:0.1mm~3.0mm
Roll width:1m~8m  Roll length:50m~100m
Color:Black or at your request
Density: 0.94g /cm3
Temperature range: -60oC -- +60oC
Life time: more than 50 years
Executive standard: GB/T 17643-2011

Main Features of EVA,HDPE,LLDPE,PVC,LDPE Material HDPE geomembrane:

 1.Long life, anti-aging, roof material can be more than 20 years, underground can be more than 50 years.

 2. Good tensile strength, high elongation.

 3. Good high/low temperature flexibility

 4.Easy to construct, no pollution.

 5. Good anti-corrosive ability, can be used in special area

6.Various colors are available

 

Specifications of EVA,HDPE,LLDPE,PVC,LDPE Material HDPE geomembrane:

 

 

NO

 

Item

                                    Value
0.75mm1.00mm1.25mm1.50mm2.00mm2.50mm3.00mm
1Density (g/cm2)0.939
2Tensile propeties
Yield strength (N/mm)    11    151822293744
Break strength (N/mm)20273340536780
Yield elongation (%)12
Break elongation (%)≥450
3Tear resistance (N)93125156187249311374
4Puncture resistance (N)240320400480640800960
5Stree crack tensistance (h)≥1500
6Carbon black
Carbon black content (%)2.0-3.0
Carbon black dispersionCarbon black dispersion   (only near spherical agglomerates)fo r10 different
views 9 in categories 1   or 2 and 1 in category3
7Oxidative induction time(OIT)
Standard OIT(min)100
High pressure OIT(min)400
8Oven aging at 85°C
Standard OIT-% retained after 90 days (%)55
High pressure OIT-% retained after 90 days (%)80
9UV Resistance
Standard OIT retained after 1600 hrs (%)50
High pressure OITretained after 1600 hrs (%)50
10Low tempreture impact brittle property at -70°CPass
11Premeability ( g.cm/(cm2).Pa)1.0×10-13
12Dimensional stability (%)±2


Applications of EVA,HDPE,LLDPE,PVC,LDPE Material HDPE geomembrane:

1.Prevent leakage disposal in waste burying field or waste water or waste dregs disposing field,river bank,lake dam ,mine remainings ,reservior,tunnel,liquid storage ,pool(pit,mine)

2.Preventing leakage in subway ,basement,tunnel ,hole

3.Anti-solt leakage in roadbed and other groundtill

4.The plane direction laying of dam ,the vertical direction laying fou groundtill ,used in the construction fence and waste material field

5.Used in seawater or freshwater feed field

6.Used in groundtill of road,highway ,railway and waterproof layer of swelling clay  and wet collapsed loess

Preventing leakage on rooftop.

 

IMages of EVA,HDPE,LLDPE,PVC,LDPE Material HDPE geomembrane:


Geomembranes Type and EVA,HDPE,LLDPE,PVC,LDPE Material HDPE geomembrane for lake liners

 

Geomembranes Type and EVA,HDPE,LLDPE,PVC,LDPE Material HDPE geomembrane for lake liners 

Geomembranes Type and EVA,HDPE,LLDPE,PVC,LDPE Material HDPE geomembrane for lake liners


 

FAQ:

1. Do you supply free samples for customers?

Yes,we will supply free samples for you.Please send your address for us.

2. How Many years experience do you have?
We have been exported to more than 20 countries in the past 15 years.

3. How long do we usually reply your request?

We always reply our customer within 24 hours.

 

Send a message to us:

Remaining: 4000 characters

- Self introduction

- Required specifications

- Inquire about price/MOQ

Q:How to lay the waterproof geotechnical membrane?
Q:Geomembrane, HDPE film in the garbage disposal field when the application of what kind of thickness can choose? How to choose?
Under normal circumstances in the country, landfill geomembrane design is 1.5 mm geomembrane, 5000 g bentonite waterproof blanket, 600 g filament geotextile.
Q:How long can glass sound insulation film be used?
It usually can be used for around 1.2 years.
Q:How to choose the geomembrane?
You should try to choose imported geomembrane. The domestic geomembrane all uses reused materials, which has a great impact on the life of the geotechnical membrane. The materials and production process control of the geomembrane are much better. The geomembrane of Canadian Soma (Solmax) which is the largest geotechnical membrane manufacturers all over the world. You can go online to search it.
Q:How to install the electric heating film?
It can be installed under the floor when decorating the house. It can begin to work when temperature control is intalled by groups parallel connection method. Of course, it is quite simple when saying it. It is better to ask a professional company to install this kind of electric products for you. First, you can fix the baseboard and then put insulating layer with reflective film and electrothermal film on it. In the final step, you can install some bamboo curtain splints or decorate fabric with good heat dissipation.
Q:Is it necessary to stick film for ipad?
No, it is not necessary. You had better to stick film so that your ipad will be not easily scratched. The film basically has three kinds: 1. The HD and transparent film looks like no film. When you are calling, your phone will close to your face and you will feel a bit greasy. 2. The frosted film looks like a bit fuzzy, but does not affect the use. At the first, you may be not accustomed, but after a long time, you will be accustomed. The biggest difference between this film and high-definition film is that it is dry, and you won't feel greasy when you touch it. 3. Diamond film There is some so-called sparkled diamond fragments in it. But whether there is diamond fragment, has not been studied. It is the same as high-definition film, feeling a bit greasy.
Q:What's the question need to notice about the construction method of composite geo-membrane?
Before laying HDPE geomembrane, there should be qualified acceptance documents of civil engineering. 2. Before cutting HDPE membrane, its size should be accurately measured, and then cutting according to the actual size, it commonly should not be cut according to the actual size but should be numbered one by one, and be detailedly recorded on the special form. 3. When laying HDPE geomembrane, welding line quantity should be controled, on the premise of guaranteeing quality, we should try best to save raw materials. At the same time, it's easy to ensure the quality. 4. The joint width of seam between film and film is generally more than 10 cm, usually make the welding line direction parallel to the maximum gradient, namely along the gradient direction. 5. Usually, in a corner and abnormal section, seam length should be shorten as far as possible. In addition to the special requirements, in slope greater than 1: Within the scope of 1.5 meters away from the slopes top or the stress concentration area, welding line should not be set up as far as possible. 6. While laying HDPE geomembrane, in order to avoid artificial fold, when the temperature is lower, we should try to tighten, paving the film. 7, after paving the HDPE geomembrane, walking or moving tools on the film should be avoided as far as possible, the things that will danger the HDPE geomembrane should not be placed on the fil, or carried while walking on the film, to avoid the accidental harms.
Q:What are the specifications of moistureproof membranes?
Common moistureproof membranes include wallpapers, coating layers, plywood. Professional moistureproof membranes are developed by water technology which are harmless to the human body and the environment for no volatilization of polluting gases. Comparing with the traditional oil alkyd varnish, it effectively protect the indoor environment.
Q:What exactly is the geomembrane? What are the applications?
At the same time, alkali and salt corrosion, long service life; and non-woven fabric is also a kind of high-molecule short fiber chemical material. Geomembrane construction site its main mechanism is to use imperviousness of plastic film to cut off earth dam leakage passage, not only increases the tensile strength and anti-puncture ability of plastic film. They have good corrosion resistance to bacteria and chemical action, which is conducive to the stability of composite geomembrane and protective layer, with high tensile strength and extensibility, bearing the hydraulic pressure and adapting to dam deformation with its large tensile strength and ductility, increasing the friction coefficient of the contact surface. And due to the roughness of the non-woven surface, geomembrane construction site its main mechanism is to use imperviousness of plastic film to cut off earth dam leakage passage; and non-woven fabric is also a kind of high-molecule short fiber chemical material, bearing the hydraulic pressure and adapting to dam deformation with its large tensile strength and ductility, through needle punching or hot sticking forming, it is combined with plastic film, used in the dark place, not afraid of acid
Q:Imported geomembrane imported anti seepage film width.
Now imported geomembrane 8 meters in width before we make drainage network.the length of Jianasuoma imported geomembrane is 8 meters in a bidding.

1. Manufacturer Overview

Location
Year Established
Annual Output Value
Main Markets
Company Certifications

2. Manufacturer Certificates

a) Certification Name  
Range  
Reference  
Validity Period  

3. Manufacturer Capability

a)Trade Capacity  
Nearest Port
Export Percentage
No.of Employees in Trade Department
Language Spoken:
b)Factory Information  
Factory Size:
No. of Production Lines
Contract Manufacturing
Product Price Range