Multicolored Slate Flake is surfacing material for SBS/APP modified bitumen waterproofing membrane and asphalt shingle. The slate flake and granules can protect the membrane and shingle and extend their service life. Since these materials have different colors, they can make the membrane and shingle more colorful.
Technical Data of Multicolored Slate Flake:
Item |
Description |
Mesh |
Tons/20Fcl |
C01 |
Dark green |
8-40 |
20 |
C02 |
Light green |
8-40 |
20 |
C03 |
Dark red |
8-40 |
20 |
C04 |
Maroon |
8-40 |
20 |
C05 |
Bright red |
8-40 |
20 |
C06 |
Pink |
8-40 |
20 |
C07 |
Dark blue |
8-40 |
20 |
C08 |
Blue |
8-40 |
20 |
C09 |
Light blue |
8-40 |
20 |
C10 |
Yellow |
8-40 |
20 |
C11 |
Orange |
8-40 |
20 |
C12 |
Khaki |
8-40 |
20 |
C13 |
Black |
8-40 |
20 |
C14 |
Grey |
8-40 |
20 |
C15 |
White |
8-40 |
20 |
Package of Multicolored Slate Flake:
Each ton is put into one PP woven bag, and then put onto one wooden pallet, 20MT are loaded into 1*20FCL. Based on order quantity, special package is available.
- Q: What is the impact of TPO waterproofing membrane welding performance?
- Factors affecting the welding performance of TPO coil mainly in the following areas: 1. Material melting point and welding window;
- Q: Waterproof electrode, waterproof welding
- 3, the more the more welding when the weld, the better the location, until the leak attributed to a little. At this time according to the size of the overflow pressure can be used in different ways: 1, with a tap into the cone of the welding plug, such as holes, temporarily blocked the hole, and then welding. 2, if the hole small, but the water more urgent. At this time may wish to elongate the arc, the use of electric home hot hole around the baked, the use of peripheral metal heat expansion, temporary swelling of the pores or simply hammer the hole immediately after the welding. Require this spot welding to be quick and accurate. When the droplets will be blocked after the hole, immediately off the arc. Action to be fast, so that the droplets have been blocked quickly cooled and completed welding. If the arc is too slow, then the back of the droplets have been re-melting, re-blowing under pressure. To be a little at the hole after the cooling, according to the need for re-welding.
- Q: Surfacing isolation layer is the application of what, how to achieve surfacing isolation layer weld.
- In order to maximize the role of the surfacing layer, the desired surfacing method has a smaller base metal dilution, higher welding speed and excellent surfacing performance, ie high quality, high efficiency, low dilution of the surfacing technology.
1. Manufacturer Overview
Location | Beijing, China |
Year Established | 2002 |
Annual Output Value | Above 1.0 Billion RMB |
Main Markets | Europe; North America; Middle East; Southeast Asia |
Company Certifications | ISO 9001 |
2. Manufacturer Certificates
a) Certification Name | |
Range | |
Reference | |
Validity Period |
3. Manufacturer Capability
a) Trade Capacity | |
Nearest Port | Tianjin |
Export Percentage | 10% - 20% |
No.of Employees in Trade Department | Above 10 people |
Language Spoken: | English; Chinese |
b) Factory Information | |
Factory Size: | Above 3000 square meters |
No. of Production Lines | Above 10 |
Contract Manufacturing | OEM Service Offered; Design Service Offered |
Product Price Range | Negotiated |
Send your message to us
Multicolored Slate Flake
- Loading Port:
- China Main Port
- Payment Terms:
- TT or L/C
- Min Order Qty:
- 1*20'FCL m.t.
- Supply Capability:
- 100 Tons per Month m.t./month
OKorder Service Pledge
OKorder Financial Service
Similar products
Hot products
Hot Searches
Related keywords