• O seals Neoprene O ring Neoprene O seal Neoprene O gasket Neoprene seal gasket System 1
  • O seals Neoprene O ring Neoprene O seal Neoprene O gasket Neoprene seal gasket System 2
  • O seals Neoprene O ring Neoprene O seal Neoprene O gasket Neoprene seal gasket System 3
O seals Neoprene O ring Neoprene O seal Neoprene O gasket Neoprene seal gasket

O seals Neoprene O ring Neoprene O seal Neoprene O gasket Neoprene seal gasket

Ref Price:
get latest price
Loading Port:
Tianjin
Payment Terms:
TT OR LC
Min Order Qty:
500 pc
Supply Capability:
5000000 pc/month

Add to My Favorites

Follow us:


OKorder Service Pledge

Quality Product, Order Online Tracking, Timely Delivery

OKorder Financial Service

Credit Rating, Credit Services, Credit Purchasing

Specifications

Silicone O Ring,Viton O Ring,Rubber O Ring 
1.Mould:More 5000 
2.Best price and high quality 
3.Certificate:ISO9001-2000,TS16969

Silicone O Ring,Viton O Ring,Rubber O Ring

Viton O ring.

Abbreviation :FKM

Common Name :Fluoro Elastomers

ASTM D-2000 classification:HK

Military(Mil-Std417) :MIL=R-25897/MIL-R-83248

Chemical Definition :Fluorinated Hydrocarbon

Durometer-Range (Shore A) :60-90

Tensile Range (P.S.I) :500-2000

Elongation (Max.%) :300

Compression Set:Good

Resilience-Rebound:Fair

Abrasion Resistance:Good

Tear Resistance:Good

Solvent Resistance:Excellent

Oil Resistance:Excellent

Low Temperature Usage (°F:+10° to -10°

High Temperature Usage (°F) :400° to 600° (depending on time and service condition)

Aging Weather- Sunlight:Excellent

Adhesion To Metals:Good

Advantage:

1. Heat resistance up to 600°F

2. Resistance to wide range of oils and solvents; specially all aliphatic, aromatic and halogenated hydrocarbons, acids, animal and vegetable oils.

Disadvantage:

1. Not recommended for ketones, low molecular weight esters and nitro containing compounds.

Usage:

Automobile,motorcycle,diesel engine,and fuel system


Silicone O ring.

Abbreviation :silicone

ASTM D-2000 classification:FC,FE,CE

Military(Mil-Std417) :TA

Chemical Definition :polysiloxane

Durometer-Range (Shore A) :30-90

Tensile Range (P.S.I) :200-1500

Elongation (Max.%) :700

Compression Set:Good

Resilience- Rebound:Good

Abrasion Resistance:Fair to poor

Tear Resistance:poor

Solvent Resistance:poor

Oil Resistance:Fair to poor

Low Temperature Usage (°F:-60° to -150°

High Temperature Usage (°F) :450°

Aging Weather- Sunlight:Excellent

Adhesion To Metals:Good

Advantage:

1.after modulating formula, the tensile strength up to 1500 psi, and tear resistance up to 88 LBS.

2.Good elasticity and good compression deformation.

3.good resistance to neutral solvent.

4.excellent heat resistance.

5.With excellent cold resistance.

6.with excellent resistance to erosion of ozone and oxides .

Disadvantage:

1.Does not recommend is suitable for most concentrated solvent, oil, concentrated acid after dilute sodium hydroxide

Usage: 

Appliance:electric kettle,electric iron,Microwave owen,etc

 

Keypad,heat shock in DVD,cable connector

 

 Silicone O Ring,Viton O Ring,Rubber O Ring

 

 Silicone O Ring,Viton O Ring,Rubber O Ring

NBR O ring.

Abbreviation: NBR

Common Name:Buna N, Nitrile, NBR

Chemical Definition:Butadiene Acrylonitrile

General Characteristics:Waterproof,oilproof

Durometer-Range (Shore A):20-95

Tensile Range (P.S.I):200-3000

Elongation (Max.%):600

Compression Set:Good

Resilience-Rebound:Good

Abrasion Resistance:Excellent

Tear Resistance:Good

Solvent Resistance:Good to Excellent

Oil Resistance:Good to Excellent

Low Temperature Usage (°F):-30° to - 40°

High Temperature Usage (°F):to 250°

Aging Weather-Sunlight:Poor

Adhesion To Metals:Good to Excellent

Usual Hardness range:50-90 shore A

Advantage:

1. Has good solvent, oil, water and hydraulic fluid resistance.

2. Good compression set, abrasion resistance and tensile strength. 

Disadvantage:

1. Not recommended for using in highly polar solvents such as acetone, and MEK, ozone, chlorinated hydrocarbons and nitro hydrocarbons.

Usage: fuel tank, grease-box, hydraulic, gasoline, water, silicone oil, etc

 

HNBR O ring.

Abbreviation:HNBR

Common Name:HNBR

Chemical Definition:Hydrogenated AcrylonitrileButadiene

General Characteristics:abrasion, compression set, tensiles

Durometer-Range (Shore A) :50-90

Tensile Range (P.S.I) :2600

Elongation (Max.%):530

Compression Set:Excellent

Resilience- Rebound:Excellent

Abrasion Resistance:Excellent

Tear Resistance:Excellent

Solvent Resistance:Good

Oil Resistance:Excellent

Low Temperature Usage (°F) :-65° to 250°

High Temperature Usage (°F) :to 350°

Aging Weather- Sunlight:Excellent

Adhesion To Metals:Good

Usual Hardness range:60-80 shore A

Usage: Fridge,automobile engine,etc

 Silicone O Ring,Viton O Ring,Rubber O Ring

 

Silicone O Ring,Viton O Ring,Rubber O Ring

EPDM O ring.

Abbreviation:EPDM

Common Name:EPR, EPT, EPDM

ASTM D-2000 classification:CA

Military(Mil-Std417) :RS

Chemical Definition:Ethylene Propylene

Durometer-Range (Shore A) :30-90

Tensile Range (P.S.I) :500-2500

Elongation (Max.%) :600

Compression Set :Good

Resilience-Rebound :Good

Abrasion Resistance:Good

Tear Resistance:Fair

Solvent Resistance:Poor

Oil Resistance:Poor

Low Temperature Usage (°F) :-20° to 60°

High Temperature Usage (°F):to 350°

Aging Weather- Sunlight:Excellent

Adhesion To Metals:Fair to Good

Usual Hardness range:50-90 shore A

Usage: Sanitary ware; brake; radiator

 

 

Silicone O Ring,Viton O Ring,Rubber O Ring

NR O ring.

Abbreviation:NR

Common name:Nature Rubber

ASTM D-2000 classification:AA

Military(Mil-Std417) :RN

Chemical Definition :polyisoprene

Durometer-Range (Shore A) :20-90

Tensile Range (P.S.I) :500-3500

Elongation (Max.%) :700

Compression Set:Excellent

Resilience- Rebound:Excellent

Abrasion Resistance:Excellent

Tear Resistance:Excellent

Solvent Resistance:Poor

Oil Resistance:Poor

Low Temperature Usage (°F:-20° to -60°

High Temperature Usage (°F) :to 175°

Aging Weather-Sunlight:Poor

Adhesion To Metals: Excellent

Usual Hardness range:35-80 shore A

 



Neoprene O ring.

Abbreviation :Neoprene

ASTM D-2000 classification:BC,BE

Military(Mil-Std417):SC

Chemical Definition :polychloroprene

Durometer-Range (Shore A) :20-95

Tensile Range (P.S.I) :500-3000

Elongation (Max.%) :600

Compression Set:Good

Resilience- Rebound:Excellent

Abrasion Resistance:Excellent

Tear Resistance:Good

Solvent Resistance:Fair

Oil Resistance:Fair

Low Temperature Usage (°F:+10° to -50°

High Temperature Usage (°F) :to 225°

Aging Weather- Sunlight:Good

Adhesion To Metals:Good to Excellent

Usal Hardness range:50-90 shore A

 Silicone O Ring,Viton O Ring,Rubber O Ring


Q:Why does Richell Richell plastic cups have a washer?
This is the unique double leak proof design of Richell. They have plastic drinking cups.
Q:I would like to ask how that kind of sealing gasket is made and processed. That's the kind of gasket that is thin in the bottle lid. What kind of PE material can be worked out with a machine and a grinding tool? ~ thank you ~!
That's good. I know that. I just don't know what the machine is made of. Can you explain it in detail?Chasing the answerThere is a press, you go to the machinery factory to ask, you know
Q:The outer ball tooth ring sensor mud suede cover gasket what use to send
In the light seal, as well as the use of rubber bellows as an auxiliary seal, rubber bellows elastic limited, generally need to be supplemented with spring to meet the loading elasticity. Mechanical seals are often referred to as "mechanical seals"".
Q:What's the difference between a sealing washer and an elastic washer?
For example, belts are divided into A, B, C, D, O belts. In fact, it is used for sealing. Usually you go to the seller's shop and he can help you figure out what you need. Not as good as uncertainty, preferably with drawings or objects in the past to buy.
Q:Why is copper gasket always leaking out of the sealing surface?
The sealing surface of two different material substances in contact is generally cast iron, cast iron due to the thermal expansion coefficient of copper with different period of time when the heating operation of the equipment, will not leak in a short time, but when the device stops again after operation will be oil leakage.
Q:How can I remove the stains from the rubber washer on the blender? How can I remove the stains from the rubber washer on the blender? Because it is the entrance, so I dare not use 84 disinfectant.
Use a toothbrush, add toothpaste, scrub, rinse with salt water!
Q:The plastic flange diameter 500, tried polytetrafluoroethylene PTFE gasket, sealing tape, but are unable to achieve the ideal sealing! Find the material that is resistant to hydrofluoric acid to be used as gasket! The test pressure is 2 kg!
Kunming Economic Development Zone, the morning fluorine plastic factory plastic experts to answer as follows: your larger diameter, but the pressure is not big, PTFE itself is one of the most corrosion resistant material, so the choice of PTFE material right, you should be made into thin gaskets, washers, must be modified to PTFE, reduce creep
Q:What are the advantages and disadvantages of those materials and materials used in the air compressor GASKET? FiveIncluding a number of commonly used non-metallic gaskets, what is the specific material name?
Non-metallic gasket materials are: graphite composite pad, is characterized by high temperature, oil resistance, corrosion resistance. Asbestos gaskets are widely used in petrochemical industry. Rubber gaskets, insulation, corrosion resistance, good sealing performance, PTFE gasket features. Known as "plastic king", insulation, corrosion resistance, non-toxic applications, medicine, food and so on. These are commonly used non-metallic gasket, compressed air gasket gasket generally choose asbestos, PTFE problems, ++369643049 ha ha
Q:The engine cover, or valve cover, cylinder head cover, the cover is the engine.This is my graduation project... The NASTRAN is used, but the rest of the software is basically the same.Hope to have experienced master Zhidianmijin ah.At present, only 12 order free modal analysis is performed. The final is to do static strength, sealing. The details of the process are not clear. For example, how does the bolt hole bind? Does it hold all the points on the inside surface? What about the boundary conditions and loading? It has more than ten bolt holes, one ring gasket, and 120 0.7bar pressure inside. The material is engineering plastics.Or some people know the whole process from modeling to the results of the general steps to say, you can, thank you first. OK, add more. StopFrequency response and transient response are currently being done
You have a lot of problems in this, and other people to advise you, it is also quite troublesome ah. I suggest that I try my best, try some specific questions and ask questions, so it will be better!
Q:Gasket, packing belongs to the scope of mechanical seals?
Gaskets and packings are sealed, but they are not mechanical seals

1. Manufacturer Overview

Location
Year Established
Annual Output Value
Main Markets
Company Certifications

2. Manufacturer Certificates

a) Certification Name  
Range  
Reference  
Validity Period  

3. Manufacturer Capability

a)Trade Capacity  
Nearest Port
Export Percentage
No.of Employees in Trade Department
Language Spoken:
b)Factory Information  
Factory Size:
No. of Production Lines
Contract Manufacturing
Product Price Range

Send your message to us

This is not what you are looking for? Post Buying Request

Similar products

New products

Hot products


Hot Searches

Related keywords