Product Description:

Tinplate for Caps Use With High Quality

1.Structure of Description

Tinplate for Caps Use With High Quality is one of the metal packing materials, which is widely used for making painting cans ,chemical package cans , electrical cable ,battery and metal printing etc.

2. Main Features

Steady and high quality

Fast shipment

Good experience for export work

Price competitive

Good payment term

Safe Package

3. Images

 Tinplate Sheet for Caps Use With High Quality

4. Specification

 

Standard : GB2520-2000 ,JIS G3303

Steel type : SPCC,MR

Coating : 2.8/2.8

Surface: Bright, Stone ,

Thickness:0.31

Annealing: CA,BA

Width :600MM~1000MM

Temper : T1~T5,DR8

Package: tinplate wrapped completely with an inner cover of plastic or waterproof papers with vorners protected with metal angels.

 

5.FAQ

A. What is the package of tinplate? (Referred as below)

For sheets, thin plastic film + rust-proof paper + metallic cover + metallic angles+ steel band strips + fumigated wooden pallet.

For coil, thin plastic film + rust proof paper + metallic cover + steel band strips + fumigated wooden pallet

Send a message to us:

Remaining: 4000 characters

- Self introduction

- Required specifications

- Inquire about price/MOQ

Q:Why do tin tins rust easily when they are opened?
The tinplate is of poor quality and the tin is not enough
Q:What are the causes of tinplate rusting and how to prevent them?
Invasion of water. The water is on the iron sheet to form a galvanic cell. This should keep the environment dry. Besides, the temperature difference between the iron sheet and the environment should not be too great to avoid the moisture in the air falling out on the sheet iron.
Q:How do you solve the water stains on the tinplate?
The root damage is caused by waterlogging, and the transport of water and nutrients is a problem. Of course, the unnecessary dead leaves are cut off
Q:What do tinplate do?
If is a tin factory, then electroplating factory, the process is open book, roll up, cold rolled plate by welding, looper, alkali washing, acid pickling, tin plating, soft melting, chemical treatment passivation, oiling and rewinding.
Q:What material is the tin plate, please?
Popularly speaking, it was tin plated on the surface of the iron sheet, just because it was imported by Macao at that time, so it always called "tinplate iron"
Q:Tin, tin plated iron. Why can't we get white wine?
Passivation of the tinplate, if further coating, will be very good corrosion resistance, but these coatings are not resistant to alcohol.In short, tinplate is afraid of water, but also afraid of alcohol, so it can not be loaded white wine.
Q:What is the difference between Maguchi Tetsu tinplate and galvanized board
Zinc plating on the surface of thin steel plates and steel strips by continuous hot dip plating prevents corrosion of the surface of thin steel plates and steel strips. Galvanized steel sheet and steel strip are widely used in machinery, light industry, construction, transportation, chemical industry, post and telecommunications and other industries.
Q:You can do is tin iron electromagnet
Tinplate is a tin covered with tin, it is not easy to rust, also known as tin iron.
Q:A tin rust problem for help
If the cooling water contains more impurities and negative ions, the sterilization process will lead to an electrochemical reaction. The impurity anion will form a galvanic cell between the Fe at the damage of the coating of the tank, which will lead to rust.
Q:Who can tell me how to adjust the roller seal defects?
In the sealing device, the roll sealing roller, the upper pressure head tray, usually referred to as sealing three elements. The correct groove shape of the roller, the reasonable position of the head and the proper driving force of the tray support are the necessary conditions to ensure the normal roll sealing. (see Fig. 1) it is easy to see that the three elements of the seal are the basic components of the sealing device and are also a fundamental factor affecting the double hemming.

1. Manufacturer Overview

Location
Year Established
Annual Output Value
Main Markets
Company Certifications

2. Manufacturer Certificates

a) Certification Name  
Range  
Reference  
Validity Period  

3. Manufacturer Capability

a)Trade Capacity  
Nearest Port
Export Percentage
No.of Employees in Trade Department
Language Spoken:
b)Factory Information  
Factory Size:
No. of Production Lines
Contract Manufacturing
Product Price Range