Specifications of Lithopone B311
LITHOPONE B311 28-30% Standard GB/T1707-1995
Total amount of zinc(calculated as Zinc Sulfide) %≥99
Total amount of Zinc (calculated as Zinc sulfide) %≥28
Zinc oxide %≤0.3
Volatile matter at 105 %≤0.3
Matter solube in water %≤0.3
Reside on sieve %≤0.1
Color(Comparing with standard sample) better
Alkalinity of the aqueous extractneutral 6-8
Oil absorption value, g/100g ≤10
Color elimination power (Comparing with standard sample) %≥105
Hiding power (Comparative ratio) %≥-5
3. Origin: China
4. Packing: in 50kg/bag in pp (net weught)
TDS of Lithopone:
Item | Index | |||||
Best quality | First quality | Qualifier | Best quality | First quality | Qualifier | |
Total zinc(ZnS) and Barium sulfate, %(m/m) ≥ | 99 | 99 | ||||
Totla zinc (ZnS), %(m/m) ≤ | 30 | 28 | ||||
Zinc oxide, %(m/m) ≤ | 0.6 | 0.8 | 1 | 0.3 | 0.3 | 0.5 |
105°C volatiles, %(m/m) ≤ | 0.3 | 0.3 | 0.5 | 0.3 | 0.3 | 0.5 |
Water insolubles, %(m/m) ≤ | 0.4 | 0.5 | 0.5 | 0.3 | 0.4 | 0.5 |
Residue on sieve (63 µm ), %(m/m) ≤ | 0.1 | 0.1 | 0.1 | 0.1 | 0.1 | 0.1 |
Color (compared with standard sample) | Better | Near | Slightly worse | Better | Near | Slightly worse |
Alkalinity of water extract | Neutral | Neutral | Neutral | Neutral | Neutral | Neutral |
Oil absorption, g/ 100g ≤ | 14 | 10 | ||||
Color dint ( compared with standard sample), % ≥ | 105 | 100 | 95 | 105 | 100 | 95 |
Hiding power | No lower 5% of standard sample | No lower 5% of standard sample |
Storage of Lithopone:
Keep the product unstacked in dry and closed rooms at normal temperature and air humidity.
To achieve best possible results, we recommend storage under the conditions stated above and use within 12 months from delivery.
- Q:Im 6 months pregnant and we are gonna paint the house.what is the best and safe wall paint brand to use??. Please, any advise????
- just make sure there are plenty of windows open when you are painting, and you should be fine.
- Q:Lithium-ion polymer battery low temperature how much work '
- Ordinary lithium-ion polymer battery discharge operating temperature range is -20 to 60 degrees, special can reach -30 degrees. Under the insulation of the battery can release the power of only the normal capacity of about 70% -80%.
- Q:Does it oxidize or dry i know that oil paint oxidizes but does nail polish and paint do too?
- Oxidize? You mean rust? Oil paint doesn't rust.
- Q:60 square meters of the house to use the number of paint and paint
- The coating area of the latex paint depends on the flatness of the substrate and the coating rate of the paint itself. The coating rate is generally marked on the drum, because it is twice the brush, so dividing by 2 is the theoretical brushing area. The surface is more rough on the RBI margin, with putty approved in accordance with the theory of brushing area calculation.
- Q:What are the differences between inorganic paints and latex paints?
- Different sources: latex paint from the resin, and inorganic paint from the quartz ore.
- Q:Tattoo paint which are several kinds of
- According to the function of color materials: tattoo art pigment - for art, religious beliefs, personality and other factors or cover the scar birthmark and other purposes, in the skin on a certain area of the pattern of engraving art. Beauty repair pigment - in order to pursue the aesthetic effect of the human body, eyebrows, eyeliner, lips, areola and other parts of the local hook line coloring beauty behavior.
- Q:what is milk paint is it more exspensive then normal paint? does it have a strong odor?
- Milk okorder I have used it on some historic restoration projects. I probably would use a more modern product unless there was a real reason that milk paint was required.
- Q:Can paint be conductive?
- There is a special conductive paint that requires special ingredients.
- Q:I will be painting my bathroom this week. It has peeling paint, and some smalll patch workI know I need to remove the loose paint, but any other steps before painting, and what type of paint should I use?
- Sand then wash with TSP and rinse it very well. Repair the damage with spackle.....Then prime. Primer is really important so you don't get peeling again. As far as paint you want a paint that is made for bathrooms and kitchens. Let the paint dry thoroughly before putting on a second coat. Let the paint cure for a few days before showering in that bathroom or at least open a window and run a fan for several days after showers to get the room dry. Painting a bathroom is tricky in cold weather if you live in an area with cold weather and this is your only bathroom perhaps wait til spring.
- Q:Ms Paint
- Paint (formerly Paintbrush for Windows) is a simple graphics painting program that has been included with almost all versions of Microsoft Windows since its first release. It is often referred to as MS Paint or Microsoft Paint. The program opens and saves files as Windows bitmap (24-bit, 256 color, 16 color, and monochrome, all with the .bmp extension), JPEG, GIF (without animation or transparency, although the Windows 98 version and a Windows 95 upgrade did support the latter), PNG (without alpha channel), and TIFF. The program can be in color mode or two-color black-and-white, but there is no grayscale mode.
1. Manufacturer Overview |
|
---|---|
Location | Xinjiang, China |
Year Established | 2001 |
Annual Output Value | Above US$ 600 Million |
Main Markets | North America; South America; Eastern Europe; Southeast Asia; Africa; Oceania; Mid East; Eastern Asia; Western Europe; Southern Europ; South Asia |
Company Certifications | IS09001-2008 |
2. Manufacturer Certificates |
|
---|---|
a) Certification Name | |
Range | |
Reference | |
Validity Period |
3. Manufacturer Capability |
|
---|---|
a)Trade Capacity | |
Nearest Port | Chongqing Port |
Export Percentage | 21% - 30% |
No.of Employees in Trade Department | 10-20 People |
Language Spoken: | English; Chinese; |
b)Factory Information | |
Factory Size: | Above 20,000 square meters |
No. of Production Lines | Above 6 |
Contract Manufacturing | Design Service Offered; Buyer Label Offered |
Product Price Range | High; Average |
Send your message to us
Lithopone B311
- Loading Port:
- Tianjin Port
- Payment Terms:
- TT or LC
- Min Order Qty:
- 24MT m.t.
- Supply Capability:
- 120000MT Per Year m.t./month
OKorder Service Pledge
OKorder Financial Service
Similar products
New products
Hot products